The utility model relates to a red brick firing process, in particular to a brick making technique. The process of using paper mill sludge instead of fly ash, slag, coal gangue; the red clay 40 - 60%, 40 - 60% paper-making sludge, after mixing, drying, drying and firing of billet and finished products from the kiln firing process, obtaining high quality brick. The invention realizes the resource utilization of waste paper sludge; reducing the amount of freight of coal gangue and fly ash or buy cost per thousand brick can be reduced into 20 - 65 yuan, greatly reducing the cost of brick; brick firing from color, intensity, sound and other elements are superior to adding powder ash composition of red brick.
【技術實現步驟摘要】
本專利技術涉及一種制磚技術。
技術介紹
目前,利用百分之百的紅粘土燒制紅磚已被列為國家限制類產業,為了節 約紅粘土資源,紅磚生產行業多釆用紅粘土摻加一定量的煤矸石、爐灰或粉煤 灰燒制紅磚,以符合國家產業政策。紅磚生產過程中,摻加一定量煤矸石、爐 灰或粉煤灰,雖然能節約一部分紅土,減少土地資源的消耗,但磚的強度有所 降低,爐渣和煤矸石在摻加于紅土之前還要進行粉碎工序,增加一定的能耗和 揚塵污染,制磚成本相應增加。
技術實現思路
為了克服現有技術的不足,本專利技術提供一種新的紅磚燒制工藝,以解決現 有技術紅磚燒制強度有所降低,耗能高,制磚成本相應增加等問題。本專利技術解決其技術為所釆用的技術方案是使用造紙污泥代替粉煤灰、爐渣灰、煤矸石,釆用紅粘土 40-60%,造紙污泥40-60%,經配料混合、制坯、晾曬 烘干、燒制、成品出窯燒制工藝,獲得高質量紅磚。釆用本專利技術的積極效果是實現了造紙污泥的廢物資源化利用;減少了粉煤 灰或煤矸石的大量運費和購買費用,每千塊紅磚可減少投入20-65元,大幅度 降低了制磚成本;燒制的紅磚從顏色、強度、聲音等要素看都要優于摻加粉煤灰等成份的紅磚。 具體實施例方式以制作紅磚1000塊為例,具體燒制工藝如下1、 配料混合取紅粘土55%,重量1.65噸,造紙干污泥45%,重量1. 35 噸,去除雜質,混合均勻備用;2、 制坯將上述混合料加水適量,經制磚機撹拌均勻,制成磚坯;3、 晾曬烘干釆用自然晾曬或機械設備烘干方式,獲得干磚坯;4、 燒制將干磚坯置入窯種高溫烘燒,與常規燒磚方式相同;5、 成品出窯;獲得高質量紅磚。權利要求1、一種紅磚 ...
【技術保護點】
一種紅磚燒制工藝,其特征是使用造紙污泥代替粉煤灰、爐渣灰、煤矸石,采用紅粘土40-60%,造紙污泥40-60%,經配料混合、制坯、晾曬烘干、燒制、成品出窯燒制工藝,獲得高質量紅磚。
【技術特征摘要】